Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Palm Labs Adhesives Turbo Anti-Seize Copper Paste TURBO ANTI-SEIZE – COPPER is a copper, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Dielectric Polymers NT-5511-2 Masking Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityHigh temperature resistantApplications: For automotive and other masking .. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP112 Low Viscosity Structural Epoxy Adhesive System Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical and.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor .. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP41S-1HTND Non-Drip, High Performance Epoxy Adhesive Description: Master Bond EP41S-1HTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a 100 to 30 mix ratio by weight and its viscosity is a smooth pas.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP75-1 Graphite Filled Electrically Conductive Epoxy System Master Bond Polymer System EP75-1 is a two component, graphite filled, electrically conductive epoxy for high performance bonding, sealing and coating formulated to cure at room temperature or more .. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond MB295 Cyanoacrylate Adhesive System Master Bond Polymer System MB295 is an ethyl cyanoacrylate adhesive system, recommended for use for combinations of plastics, lubber, ceramic or glass. Provides better general resistance to effects .. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond MB297 Cyanoacrylate Adhesive System General purpose, fills gap to 0.008Information provided by Master Bond Inc. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond SteelMaster 43HT Stainless Steel Filled Two Component Epoxy System Master Bond Steelmaster 43HT is a high performance, stainless steel filled two component epoxy resin system for the cost effective repair, maintenance, rebuilding, restoring and resealing of worn or.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond UV10TK40 UV Curable Compound Has Gap Filling Properties Description: Master Bond UV10TK40 is a higher viscosity, one part UV system for bonding, sealing and coating with good optical clarity, excellent physical properties, chemical resistance and high gl.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP34CA Low Viscosity Heat Resistant Epoxy System Master Bond EP34CA is a low viscosity, polyfunctional, heat resistant epoxy resin designed for use in high performance composite structures, potting and casting applications. EP34CA can be used up t.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP3HTS Silver Filled, Electrically Conductive Epoxy Description: Master Bond Polymer System EP3HTS is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon 910-10X##-P1 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 10 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon 920-20Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 2Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape i.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon LW201B##-P2 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon LW202R##-P0 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 2 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon LW50125Rxx-P0 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubber Cross-Se.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Arlon LW601Xxx-P1 0.060" (1.52 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Dielectric Polymers NT-511C High Temperature Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Minimum Service Temperature, Air | -51.1 °C | -60.0 °F | |
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |