Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-11® White Epoxy Paste PC-11® is a Heavy Duty-white epoxy Paste formulated by the manufacturer of PC-7.® After mixing, PC-11® can be applied to a dry, wet or underwater surface and will cure to an off white color. PC.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Protective Coating PC-Fahrenheit™ High Temperature Epoxy PC-Fahrenheit™ is a hand moldable putty epoxy designed for quick emergency-type repairs formulated for increased temperatures. PC-Fahrenheit™ can be expected to outperform other putties at high te.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Alcoa KAMA 3300 Very High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2102 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2102 C.I. is a smooth.. |
|||
Minimum Service Temperature, Air | -28.9 °C @Pressure <=1.03 MPa |
-20.0 °F @Pressure <=150 psi |
|
Garlock 244 Neoprene Rubber - Commercial Grade Soft blend of neoprene, nitrile and SBR rubbers for use as bumpers, pads, and in sealing and general gasket applications. It is not recommended in applications where high oil resistance is required.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 2564 C.I. NBR/CR/SBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2264 is a smooth fini.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 4160 Natural Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Red, smooth finishInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 50 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 567 EPDM Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish, commercial qualityInformation provided by Garlock Rubber Technologi.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock SBR Extruded Skirtboard SBR rubber extruded skirtboard for protection applicationsInformation provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Greene Tweed CHEMRAZ® 528 Perfluoroelastomer Chemraz® 528 works well in a wide variety of biotechnology and medical device applications where ling-term seal reliability is required. This seal material offers excellent performance in static.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | Approx. Cold test |
Lubriplate Shield Gear Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Applications: Open gears, normal conditions.Gear Shield Series .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 9064 Neoprene Sheet Rubber Gasketing Neoprene (CR)FDA-approved. Exceptional material for food plants, with superior resistance to most all food products; oily and aqueous.Information provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Garlock 9122 Nitrile Sheet Rubber Gasketing Nitrile (NBR)Superior resistance to aliphatic hydrocarbons, such as oil, fuels, and many types of solvents.Information provided by Garlock Rubber Technologies |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® 2819-5(R) Acrylic Adhesive Zone Tape Specification Notes: 21CFR177.1550 compliant. All data based on a 0.0047 inch test sample. Information provided by Saint Gobain Performance Products. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® 2829-3(R) Acrylic Adhesive Zone Tape Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample. Information provided by Saint Gobain Performance Products. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® K103 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M706 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain CHR® RU101 Rulon Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Rulon® films offer superior abrasion resistance when compared to conventional PTFE films. Service temperatures range from -100°F to 500°F (-73°C to +260°C). In rotating b.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain Tygon® LP 1600 Low Permeation Fuel Tubing Tygon® LP1600 Low Permeation Fuel Tubing is designed to meet new marine market emission standards. Applications Marine boats with above-deck outboard engines Personal watercraft -- Jet Skis, .. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Master Bond MB514 Hot Melt Adhesive Compound Master Bond Hot Melt MB514 is a high performance hot melt adhesive with the following key features: It is particularly suited for use on untreated surfaces of high and low density polyethylene, poly.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 2128 Clear, Light Assembly EVA Glue Stick Bostik 2128 Clear, Light Assembly EVA Glue StickClear for light assembly. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Bostik 6323 High Performance, Long Open Time EVA Glue Stick Bostik 6323 High Performance, Long Open Time EVA Glue StickLong open time. Good adhesion to metal and plastics. High performance. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | |
Saint-Gobain Furon®, Kapton® K275 Tape Description: A 1 mil thermally conductive Kapton® film, coated on both sides with 2 mils of thermally-conductive pressure-sensitive adhesive. Recommended uses: Excellent for use in small, compact e.. |
|||
Minimum Service Temperature, Air | -28.9 °C | -20.0 °F | Approx. Cold test |
Lubriplate Temp G.S. Low Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Applications: Open gears, slides, fifth wheels, low temps. Gear.. |