Material Notes:
Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2102 C.I. is a smooth-finish SBR/NBR sheet, constructed with polyester fabric.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 80
70 - 80
Tensile Strength >= 6.89 MPa
>= 1000 psi
8.96 MPa
1300 psi
Typical
Elongation at Break >= 200 %
>= 200 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F