Protective Coating PC-Fahrenheit™ High Temperature Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, High Temperature
Manufacturer Protective Coating Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Protective Coating PC-Fahrenheit™ High Temperature Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC-Fahrenheit™ is a hand moldable putty epoxy designed for quick emergency-type repairs formulated for increased temperatures. PC-Fahrenheit™ can be expected to outperform other putties at high temperatures. Temperatures extremes of 350°F (176°C) to 500°F (260°C) will reduce service life of the repair. High Temperatures contact may produce an objectionable odor. Cut, mix and apply. PC-Fahrenheit™ allows a working time of about 8 minutes and cures for service in 60 minutes. Example applications include mufflers and other auto uses, grills, stoves, steam pipes, etc.Data provided by the manufacturer.
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
1 Week Cure; ASTM D2240
Elongation at Break 1.0 %
1.0 %
Compressive Yield Strength 55.16 MPa
8000 psi
ASTM D695
Shear Strength 4.83 MPa
700 psi
Tensile Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
For Service
Pot Life 8.0 min

@Temperature 21.1 °C
8.0 min

@Temperature 70.0 °F
Working Time
Descriptive Properties Value Comments
Color Brown
Component A
Brown
Mixed
Khaki
Component B
Thermal Shock Resistance Excellent
Toxicity Nontoxic after cure