Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants 748S (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants 748S-UV (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8180 (479) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8182 (837) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8182R (837RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8190 (483) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Polikim High Density Polyethylene (HDPE) High density polyethylene is preferred when resistance to chemicals and weather is the priority. As it can be supplied in large dimensions and can be welded, its use in construction of tanks and was.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N60M Nitrile Rubber Nitrile Butadiene Rubber (NBR) 55-65 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet specification BS2751 BA60. Also meets obsolescent specification BS3.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which modulus shall not exceed 70 Mpa |
Precision Polymer Engineering N70J Nitrile Rubber Peroxide cured Nitrile Butadiene Rubber (NBR), 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet DTD 5594A standard for resistance to mineral oils.Applications: Excellent resistance i.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N70N Nitrile Rubber Nitrile Butadiene Rubber (NBR) 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet Aerospace Material Specification DTD5595A Grade 70.Applications: Synthetic rubber resistant to petrole.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Precision Polymer Engineering Z95X Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applica.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Z95X Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applica.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Butyl Rubber (IIR, CIIR, BIIR) Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and ca.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of .. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V60WH Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V90BR Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V75 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | as heat transfer fluid |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Gehman T100 |
Zeon Chemicals HyTemp® AR22 AR Super ACM Polyacrylate Elastomer Monomer composition is optimized for improved tensile strength and oil resistance over traditional acrylates. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg B939 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg Emerson & Cuming Eccobond® 104 Two-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 104 Eccobond® Two-Component High Temperature Performance Epoxy AdhesiveFilled, heat curing, high temperature resistant, epoxy adhesive. Excellent chemical resistance. Maintains hig.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Chesterton 610 MT Plus Synthetic Lubricating Fluid Description: Chesterton® 610 MT Plus Synthetic Lubricating Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from 25°C (-15°F) to those o.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Dow Corning MOLYKOTE® LONGTERM 2 PLUS High Performance Mineral Oil GreaseInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | JIS-K-6723 |
Denka REOMER G G5479 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | JIS-K-6723 |
Denka VINYKON W7100N PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants 865 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Hydrogenated Nitrile Rubber (HNBR) |