Freudenberg Simrit Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name Simriz®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of elasticity. Simriz® perfluoro elastomers close the material gap between inelastic PTFE and elastomers, which have poor temperature and chemical resistance properties. With a fluoridation level of 72%, FFKM elastomers have a level of resistance close to that of pure PTFE at 76%. At the same time, FFKM materials are so elastic that they are excellently suited to both static and dynamic seals. Simrit offers ISC O-Rings which are specifically optimised with respect to flexibility at low temperatures, resistance to high temperatures, hardness, tensile strength, elongation, compression set, or color.Information provided by Freudenburg-NOK.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Ultimate 17.1 MPa
2480 psi
Elongation at Break 260 %
260 %
Compression Set 27 %

@Temperature 200 °C
27 %

@Temperature 392 °F
70 hr
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
Descriptive Properties Value Comments
Color Black
Water Resistance 6.3
70 h; 200°C