Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -75.0 °C | -103 °F | Recommended |
Nye Lubricants UniFlor 8970 (498) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | Recommended |
Nye Lubricants UniFlor 8971 (898-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | Recommended |
Nye Lubricants UniFlor 8971R (898RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | Recommended |
Nye Lubricants UniFlor 8971S (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | |
NextGen Adhesives M907-19 Medical Grade Epoxy Adhesive Description: NGAC M907-19 is a medium viscosity and thixotropic adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include lam.. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | |
Resin Technology Group 1217 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Minimum Service Temperature, Air | -75.0 - -55.0 °C | -103 - -67.0 °F | |
Fluorosilicone Rubber (FMQ, FVMQ, FSi) Resists ozone and oxidizing chemicals, alkali, aromatic chlorinated solvents. Affected by brake fluid, ketones, and hydrazine. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | Continuous |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | as heat transfer fluid |
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | |
ATG s.r.l. PVMQ Silicone Rubber |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | |
CENTROPLAST CENTROLEN PE-HD Polyethylene high density This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor.. |
|||
Minimum Service Temperature, Air | -75.0 °C | -103 °F | temperature limit for flexibility |
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.Tygon® Ultra Chemical Resistant Tubing is virtually unaffec.. |