Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® TUT10BG3 UV Screening Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® TWH15BL3 Low Gloss White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Minimum Service Temperature, Air | -72.0 °C | -97.6 °F | Continuous |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |