Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 272 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 702A-EP (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants 795A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants PML-81 Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8170 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8170U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Recommended |
Nye Lubricants UniFlor 8172 (829) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Precision Polymer Engineering C70C Chloroprene Rubber Chloroprene Rubber, 66-75 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather. Widely used for sealing.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Precision Polymer Engineering N70H Nitrile Rubber Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene.Applications: The high acrylonitrile content of this rubber increases resist.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q50Y Polyurethane Rubber Yellow/Green Polyurethane Rubber, 50-60 °IRHD. ASTM & ISO designation = AU.Applications: Good abrasion resistance and tensile strength, with fluid compatibility approaching that of NBR. Polyuretha.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70R Polyurethane Rubber Peroxide cured, red Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion r.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering Q70X Polyurethane Rubber Peroxide cured, self-lubricating, Polyurethane Rubber, 65-75 °IRHD. Compounded with graphite or molyb-d. To meet ASTM line call-out M5BG714, B14, EO14, EO34. Polyester-based urethane. ASTM & ISO d.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Freudenberg Simrit V115 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | Retraction Temperature, TR10; ASTM D1329 |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | as heat transfer fluid |
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg B419 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg E850 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg E935 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H511 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H608 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H630 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H711 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H730 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg P600 Epichlorohydrin There are three types of epichlorohydrin:1. Homopolymers of epichlorohydrin. Designated CO.2. Chopolymers of epichlorohydrin and etylene oxide. Designated ECO.Terpolymers of epichlorohydrin, etylene.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg P650 Epichlorohydrin There are three types of epichlorohydrin:1. Homopolymers of epichlorohydrin. Designated CO.2. Chopolymers of epichlorohydrin and etylene oxide. Designated ECO.Terpolymers of epichlorohydrin, etylene.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
Trelleborg Hypalon® H606 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | See Note 1. |
ChevronTexaco MCP Grease L NLGI Grade 00 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | JIS-K-6723 |
Denka LCS Z1075 Thermoplastic Elastomer, Extrusion grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |
|||
Minimum Service Temperature, Air | -35.0 °C | -31.0 °F | |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |