Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 466 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 466 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 466 resins can be used for the following applications: adhesives, sealants.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
DuPont Bynel® 1E554 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Vicat Softening Point | 68.0 - 70.0 °C @Load 5.00 kg |
154 - 158 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds SAR 03 Rigid PVC, Antishock Injection Molding Lead Free Electric antishock fittings |
|||
Vicat Softening Point | 68.0 °C | 154 °F | A; ISO 306 |
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5023 400 Micron LDPE Powder Description: ICOFLO 510-5023 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, .. |
|||
Vicat Softening Point | >= 68.0 °C | >= 154 °F | ASTM D 1525 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 68.0 °C | >= 154 °F | ASTM D 1525 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
UBE V215 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
DuPont Appeel® LSR20D752 Lidding Sealant Resin Appeel® LSR20D752 is a modified ethylene acrylate copolymer designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ISO 306 |
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | 50N-50°C per hour; ISO 306 |
Total PPC 5752 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 5752 is a nucleated controlled-rheology heterophasic copolymer. PPC 5752 is characterized by a high impact resistance and excellent antistatic properties. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | 50N-50°C per hour; ISO 306 |
Total PPC 3640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | 50N-50°C per hour; ISO 306 |
Total PPC 3645 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3645 is a nucleated heterophasic copolymer. PPC 3645 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3645 has been devel.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | 120°C/hr, 9.8N; ASTM D1525 |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 72D727 Sealing Resin DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525, ISO 306 |
DuPont™ Elvax® 3169Z Ethylene Vinyl Acetate DuPont™ Elvax® 3169Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | B50 (50N); ISO 306 |
Domo 2340P Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | B50 (50N); ISO 306 |
Domo 2348M Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | |
BASF Novolen® 2340 P Polypropylene Grade with nucleating agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | |
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | A/50; ISO 306 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Vicat Softening Point | 68.0 °C @Load 5.10 kg |
154 °F @Load 11.2 lb |
ISO 306 |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Vicat Softening Point | 68.0 - 86.0 °C | 154 - 187 °F | Average value: 77.5 °C Grade Count:26 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | 50N; ASTM D1525 |
Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene Copolymer Polypropylene, Unreinforced, 20 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, .. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
DuPont Appeel® LSR11D625 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D625 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals .. |
|||
Vicat Softening Point | 68.0 °C | 154 °F | ASTM D1525 |
DuPont Elvax® 3169 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **) 18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Vicat Softening Point | >= 68.0 °C | >= 154 °F | ASTM D 1525 |
Karina E 837-10/68-Y-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |