Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 290 °C | 554 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7568/GY PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Superheated steam sterilizable.High chemical resistance parts, hydrolysis resistance, non .. |
|||
Vicat Softening Point | 290 °C | 554 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Vicat Softening Point | 290 °C | 554 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Vicat Softening Point | 290 °C | 554 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Vicat Softening Point | 290 °C | 554 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Vicat Softening Point | 290 °C | 554 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Vicat Softening Point | 290 °C @Load 5.10 kg |
554 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NT40 GR30 NL HS PPA, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | Average value: 290 °C Grade Count:16 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Vicat Softening Point | 290 °C | 554 °F | 50°C/h 50N; ISO 306 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |