Polymer Property : Vicat Softening Point = 430 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 221 °C
430 °F
9.8 N; ISO 306, ASTM D1525
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
Vicat Softening Point 221 °C
430 °F
120°C/h, 50 N; ASTM D1525
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Vicat Softening Point 221 °C
430 °F
120°C/h, 50 N; ASTM D1525
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Vicat Softening Point 221 °C
430 °F
120°C/h, 50 N; ASTM D1525
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Vicat Softening Point 221 °C
430 °F
B; STN EN ISO 306
Plastcom SLOVAMID 6 GF 30 Polyamide 6, 30% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
Vicat Softening Point 221 °C
430 °F
Rate A/50; ASTM D1525
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Vicat Softening Point 221 °C
430 °F
Rate A/50; ASTM D1525
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Vicat Softening Point 221 °C
430 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® V8280 PBT+PET
40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture.
Vicat Softening Point 221 °C
430 °F
Rate B/50; ISO 306
SABIC Innovative Plastics ULTEM AUT210 PEI
Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti..
Vicat Softening Point 221 °C
430 °F
Rate B/50; ISO 306
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Vicat Softening Point 221 °C
430 °F
Rate B/50; ISO 306
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Vicat Softening Point 221 °C
430 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East)
40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture.
Vicat Softening Point 221 °C
430 °F
ASTM D1525
PlastxWorld Veroplas PB3150 Nylon 66
15% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Vicat Softening Point 221 °C
430 °F
ASTM D1525
PlastxWorld Veroplas PB3300 Nylon 66
30% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
Vicat Softening Point 221 °C
430 °F
ASTM D1525
PlastxWorld Veroplas PB5300 Nylon 66
general purpose, 30% mineral filled injection molding gradeInformation provided by PlastxWorld Inc.
Vicat Softening Point 221 °C
430 °F
DAM; 50°C/h 50N; ISO 306
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..
Vicat Softening Point 221 °C
430 °F
B/50; ISO 306
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded
AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Vicat Softening Point 221 °C
430 °F
ASTM D1525
PlastxWorld Veroplas PA3300 Nylon 6
general purpose, 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc.