Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 215 °C | 419 °F | B |
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads FeaturesPBT for injection moulding, chemically reinforced with 30% glass beads. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Vicat Softening Point | 215 °C | 419 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Vicat Softening Point | 215 °C | 419 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Vicat Softening Point | 215 °C | 419 °F | VST/A/50; ISO 306 |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Vicat Softening Point | 215 °C | 419 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Vicat Softening Point | 215 °C @Load 5.00 kg |
419 °F @Load 11.0 lb |
|
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Vicat Softening Point | 215 °C | 419 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem 1010K PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 1000EF PEI Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Vicat Softening Point | 215 °C | 419 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant. |
|||
Vicat Softening Point | 215 °C | 419 °F | ISO 306 |
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Vicat Softening Point | 215 °C | 419 °F | B/50; ISO 306 |
Eurostar Staramide BG6U PA6, 30% Glass Fiber Filled, UV Stabilized, Injection Molded Staramide BG6U is an UV Stabilized, 30% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 215 °C | 419 °F | B/50; ISO 306 |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 215 °C | 419 °F | 50N; ISO 306 |
Eurotec® Tecomid® NB40 GR30 NL PA 6 30% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 215 °C @Load 5.10 kg |
419 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NB40 GR30 NL HW PA6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 215 °C @Load 5.10 kg |
419 °F @Load 11.2 lb |
ISO 306 |
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Vicat Softening Point | 215 °C | 419 °F | DAM; 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Zytel® 80G14AHS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G14AHS NC010 is a 14% glass fiber reinforced toughened high flow heat stabilized polyamide 66 resin. It offers outstanding perform.. |