Polymer Property : Vicat Softening Point = 315 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 153R PC
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release.
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® 153R PC (Asia Pacific)
Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® 4401R PPC+PC
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Lexan® 4404 PPC+PC
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® FXD153 PC
FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Co..
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® FXE154 PC
FDA compliant (color limited) PC. 2.5 MFR. Potable water/extrusion blowmoldable. ILLUMINATE special effects (fluorescent/edge glow colors).
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® HP9NR PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding ..
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Lexan® RL7517 PC
FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® FXD941A PC
FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Co..
Vicat Softening Point 157 - 205 °C
315 - 401 °F
Average value: 178 °C Grade Count:27
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
Vicat Softening Point 157 °C
315 °F
A120; ISO 306
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-6140 N is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-6140 N is developed for producing injection molded components for household eq..
Vicat Softening Point 157 °C
315 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® IQ4860HR PBT
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® IQ4860HR PBT
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Vicat Softening Point 157 °C
315 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Vicat Softening Point 157 °C
315 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Vicat Softening Point 157 °C
315 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East)
Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified.
Vicat Softening Point 157 °C
315 °F
Styron CALIBREâ„¢ 200 6 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Vicat Softening Point 157 °C
315 °F
Styron CALIBREâ„¢ 300 6 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Vicat Softening Point 157 °C
315 °F
ISO 306
Unipetrol PP MONSTEN® GB 005 Polypropylene Homopolymer
Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA
Vicat Softening Point 157 °C

@Load 5.10 kg
315 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Apec® 1697 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
Vicat Softening Point 157 °C
315 °F
Covestro Apec® HT KU 1-9333 High-Heat Polycarbonate
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Vicat Softening Point 157 °C

@Load 1.02 kg
315 °F

@Load 2.25 lb
ISO 306
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Vicat Softening Point 157 °C

@Load 1.02 kg
315 °F

@Load 2.25 lb
ISO 306
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Vicat Softening Point 157 °C
315 °F
50 N; ISO 306
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM
10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov..
Vicat Softening Point 157 °C
315 °F
50 N; ISO 306
Azoty Tarnow™ TARNOFORM 300 K POM
Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Vicat Softening Point 157 °C
315 °F
B
Plastcom SLOVALEN PH 82 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh..