Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 148 °C @Load 5.001 kg |
298 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC S75R GF20 V0 Polycarbonate, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® ML7691 PC UV stabilized clear polycarbonate formula for internal uses only. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 3010-15 Polycarbonate Resin Description: LUPOY PC 3010-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Vicat Softening Point | 148 °C | 298 °F | A120; ISO 306 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® FC 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1303-15 Polycarbonate Resin Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® F 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® FC 23 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4330-15 Polycarbonate EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Vicat Softening Point | 148 °C | 298 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 303-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 148 °C @Load 5.10 kg |
298 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV .. |
|||
Vicat Softening Point | 148 °C | 298 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 148 °C | 298 °F | ASTM D1525 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 10N-50°C per hour; ISO 306 |
Total PPH 9082 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9082 is a controlled-rheology and antistatic homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing impr.. |
|||
Vicat Softening Point | 148 °C | 298 °F | ASTM D1525 |
Total PPC 4720 WZ Polypropylene, Impact Copolymer ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated.. |
|||
Vicat Softening Point | 148 °C | 298 °F | |
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
Vicat Softening Point | 148 °C | 298 °F | |
Covestro Makrolon® KU 1-1242 Polycarbonate, High Impact High viscosity, impact modified grade with good toughness at low temperatures (light colors only).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 10 N; ASTM D1525 |
Braskem H 401 Cast Film Extrusion Polypropylene Description: H 401 is a medium melt flow rate homopolymer polypropylene, additived with slip and antiblocking agents. Designed specially for cast film. This product features good impact strength, ex.. |
|||
Vicat Softening Point | 148 °C | 298 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |