Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 127 °C @Load 1.00 kg |
261 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 706 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Films manufactured with Eraclene FA 706 show good processability t.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
SABIC B4660/B4660AB High Density Polyethylene for Blow Molding Product Description: B4660 series grades are medium molecular weight High Density Polyethylene homopolymer for blow molding applications. They are primarily designed for imparting high rigidity, t.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 127 °C @Load 5.001 kg |
261 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF2030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Chevron Phillips HiD® 9404 HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: medium molecular weight distributions, wide range of processing conditions, low parison sag, good stress crack resistance. Federal specification LP390C .. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® L5332CP High Density Polyethylene ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resis.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
LyondellBasell Alathon® M5350 High Density Polyethylene ApplicationsALATHON M 5350 copolymer with narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing s.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Europe-Africa-Middle East) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Unipetrol PE HD LITEN® VB 33 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
ExxonMobil HDPE AS55-03 High Density Polyethylene Resin Product Description: AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a good balance of stiffness and stress crack resistance.Avail.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Vicat Softening Point | 127 °C | 261 °F | 10 N; ASTM D1525 |
Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene Description: SHC7260LS-L is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. This resin has additives aga.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ASTM D1525 |
Bapolene® 2035 Polyethylene, Blow Molding Grade Bapolene HD2035 is a high density polyethylene copolymer for blow molding applications. It is recommended for applications that require high top load strength and good ESCR properties. This produc.. |
|||
Vicat Softening Point | 127 °C | 261 °F | ISO 306 |
Total Finathene® 53080 HDPE, blow molding, sheet
(discontinued **) Finathene E® 53080 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Finathene E® 53080 has been especially developed for the production of containers.. |
|||
Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |