Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Plaskolite Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 10 N - 50°C/h; ISO 306/A |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Vicat Softening Point | 90.0 - 95.0 °C | 194 - 203 °F | Average value: 92.7 °C Grade Count:3 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Eastman 18BOA Polyethylene
(discontinued **) Polyethylene 18BOA is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic mold.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.00 kg |
194 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LyondellBasell Petrothene® NA814000 Low Density Polyethylene ApplicationsPETROTHENE NA 814-000 is a low density homopolymer resin specifically developed for a wide variety of blow molding applications. This resin exhibits excellent gloss, an excellent balanc.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 50°C/h; 10N; 10x10x4mm; ISO 306/A50 |
SYNTHOS Krasten® 154 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | VST/B/50; ISO 306 |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | VST/B/50; ISO 306 |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Lubrizol Estane® CS195A Thermoplastic Polyurethane Type: Estane® CS195A is a Shore 95A, polyester grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B50 (50N); ISO 306 |
Domo 1101S Polypropylene Homopolymer Information provided by Domo. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B50 (50N); ISO 306 |
Domo 1102J Polypropylene Homopolymer Information provided by Domo. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B50 (50N); ISO 306 |
Domo 1102M Polypropylene Homopolymer Information provided by Domo. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Dow FLEXOMER™ ETS-9078 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9078 NT 7 is intended primarily for slot cast extrusion. This narrow molecular weight distribution resin has outstanding drawdown properties and produces low modulus cast films, high.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
Dow LDPE 4012M Low Density Polyethylene DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ISO 306 |
Arkema Group OREVAC® 18365 Maleic Anhydride Modified Polyethylene OREVAC® 18365 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | VST/B/50; ISO 306 |
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer This plastic is a low density, easily machined material that can be welded and has good chemical resistance. Applications include filter housings, chemical pump components and apparatus engineering.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B |
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 37% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Huntsman PE1335 EVA Film Extrusion
(discontinued **) 3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Transparent spherical pelletsFeatures: Zero halogenUses.. |