Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 81.0 °C | 178 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | Rate B; 4 mm thick;10.0 mm wide molded rod; ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | DIN 53460 |
Ineos Nova S-3400 Medium Impact Compact Polystyrene
(discontinued **) Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. For injection molding generally a lubricated type is us.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | DIN 53460 |
Ineos Nova S-3401 Medium Impact Compact Polystyrene
(discontinued **) Impact polystyrene with good flow characteristics and a high elongation. Generally used for applications where a tough material is required. The material is provided with external lubricate to imp.. |
|||
Vicat Softening Point | 81.0 - 83.0 °C @Load 5.00 kg |
178 - 181 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 325/2 Rigid PVC, Extrusion Building profiles |
|||
Vicat Softening Point | 81.0 - 83.0 °C @Load 5.00 kg |
178 - 181 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 412 Rigid PVC, Extrusion Electric channels |
|||
Vicat Softening Point | >= 81.0 °C | >= 178 °F | ASTM D 1525 |
Karina E-844-10/219-Y-ERYM White PVC Compound Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.I.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Vicat Softening Point | 81.0 - 83.0 °C @Load 5.00 kg |
178 - 181 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 321 Rigid PVC, Extrusion Lead Free Profiles |
|||
Vicat Softening Point | 81.0 - 83.0 °C @Load 5.00 kg |
178 - 181 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 320 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |
|||
Vicat Softening Point | 81.0 - 83.0 °C @Load 5.00 kg |
178 - 181 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 325 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | B120; ISO 306 |
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide.. |
|||
Vicat Softening Point | 81.0 °C @Load 5.10 kg |
178 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 416N HIPS Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su.. |
|||
Vicat Softening Point | 81.0 °C @Load 5.10 kg |
178 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 542N HIPS Styrolution PS 542N is an impact polystyrene with high heat resistance.Information provided by Styrolution |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 875A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 81.1 °C | 178 °F | ASTM D1525 |
Teknor Apex Sinvicomp SBC 3710 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
DuPont Nucrel® 0903HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment de.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSI 3630 Medium Impact Polystyrene 3630 is an easy flowing, medium impact polystyrene for injection molding. This grade offers a good compromise of flow and softening point allowing for the production of large and complex articles a.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
DuPont Nucrel® 0902HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0902HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment design.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525 |
Eastman Cadence™ GS3 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | 50°C/hr; 50N |
Polimeri Europa EDISTIR PD RK6223N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,083-12-07-23 Halogen and Antimony free, medium impact polystyrene. This grade complies at 2 mm with IEC 65-20-2 and BSI.. |
|||
Vicat Softening Point | 81.0 °C | 178 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 3135B Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3135B is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additive:.. |