Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvax® 3135B Ethylene Vinyl Acetate  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3135B Ethylene Vinyl Acetate  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Elvax® 3135B is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additive: antiblock.Applications: This resin is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown film equipment over a wide range of film thickness and blow-up ratios. It can also be coextruded with a variety of other polymers. This resin is typically used as low temperature seal layer in coextruded films.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792, ISO 1183
Vinyl Acetate Content 12 %
12 %
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 77.0 °C
171 °F
Freezing Point; ASTM D3417
97.0 °C
207 °F
ASTM D3417
Vicat Softening Point 81.0 °C
178 °F
ASTM D1525, ISO 306
Users viewing this material also viewed the following: