Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 92.0 °C | 198 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir R 540E Polystyrene HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics IS.. |
|||
Vicat Softening Point | 92.0 °C @Load 1.00 kg |
198 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® MT 40 A Linear Low Density Polyethylene Flexirene MT 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Flexirene MT 40 A is characterized by a good processability and impact r.. |
|||
Vicat Softening Point | 92.0 °C @Load 1.00 kg |
198 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MR 30 Low Density Polyethylene - Injection Molding Riblene MR 30 is a high fluidity low density polyethylene resin (LDPE) characterized by a high flowability and a medium rigidity.Parts made with Riblene MR 30 are characterized by good mechanical an.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C7122 PC+ABS (Asia Pacific) Cycoloy*C7122 is a mineral filled, non-halogenated flame retardant PC/ABS. Good stiffness with balanced flow and impact performance. |
|||
Vicat Softening Point | >= 92.0 °C | >= 198 °F | ASTM D1525 |
NIZHNEKAMSKNEFTEKHIM 524B General Purpose Polystyrene Polystyrene intended to produce glossy coating by co-extrusion. A specialty recipe provides for drastic reduction of buildup in a die plate and of streaks on an article in molding.Information provi.. |
|||
Vicat Softening Point | >= 92.0 °C | >= 198 °F | ASTM D1525 |
NIZHNEKAMSKNEFTEKHIM 825E High Impact Polystyrene Grade 825E is a high impact polystyrene designed specifically for extrusion and thermoforming. It is used for production of industrial packaging via deep draw thermoforming and custom multilayer sh.. |
|||
Vicat Softening Point | >= 92.0 °C | >= 198 °F | ASTM D1525 |
NIZHNEKAMSKNEFTEKHIM 825ES High Impact Polystyrene Grade 825ES is a high impact polystyrene designed for extrusion and hot molding application. It is suited for hot molded deep drawn industrial packages and multilayer shaped sheet production via ex.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D 1525 |
NOVA Chemicals Sclair® 31G Butene Copolymer LLDPE Extrusion Coating Resin 31G complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 31G is su.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | 50°C/h 50N; ISO 306 |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Chevron Phillips Marlex® 1409 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Eastman E6838-902F Polyethylene Film
(discontinued **) Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business .. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Eastman E6838-913P Polyethylene
(discontinued **) Polyethylene E6838-913P natural is a specialty formulation suggested for high-speed extrusion coating applications. E6838-913P offers improvements over standard low-density polyethylene in adhesion .. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Vicat Softening Point | 92.0 - 94.0 °C | 198 - 201 °F | ASTM D1525 |
Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
LyondellBasell Petrothene® NA216000 Low Density Polyethylene ApplicationsPETROTHENE NA 216-000 is a general purpose, heavy and medium weight coating resin, capable of coating weights down to 7.0 lbs/ream at line speeds of 1200 ft/min. It can be applied to pa.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5072 1200 Micron LLDPE Powder Description: ICOFLO 510-5072 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Hannam Chemical Hanalac 795 ABS, Pipe Grade Designed for pipe and bobbin sleeves. Excellent processability and high impact strength. Manufactured to prevent static electricity. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Lushan RF1000 Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene DescriptionCP 763-01 is an extruded, blow molding, and injection molding grade of low density polyethylene having good processability and heat sealability. ApplicationCP 763-01 meets the specificat.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
A. Schulman CP775-01 Molding Grade, Low Density Polyethylene DescriptionCp 755-01 is a molding grade, low-density polyethylene. ApplicationCP 755-01 meets the specification contained in FDA Regulation 177.1520 for food contact applications.Information provid.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 20% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | |
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade Grade for injection molded parts. Also available as a special grade for fibers (short spinning) and cast film.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Eastman D4041-P Polyethylene
(discontinued **) Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in an.. |
|||
Vicat Softening Point | 92.0 °C | 198 °F | ASTM D1525 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |