Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 195 °C | 383 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Vicat Softening Point | 195 - 250 °C | 383 - 482 °F | Average value: 208 °C Grade Count:57 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Vicat Softening Point | 195 °C @Load 5.00 kg |
383 °F @Load 11.0 lb |
|
LATI Laticonther 62 GR/50 PA 6, 50% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Asia Pacific) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Asia Pacific) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Vicat Softening Point | 195 °C | 383 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® SHF4960 PBT Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Vicat Softening Point | 195 °C | 383 °F | 10 N - A method; ISO 306 |
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |