Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 128 °C @Load 1.00 kg |
262 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Eraclene® MP 90 C High Density Polyethylene - Injection Molding Eraclene MP 90 C is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a high .. |
|||
Vicat Softening Point | 128 °C @Thickness 4.00 mm |
262 °F @Thickness 0.157 in |
Rate A; 10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Reliance Industries Relene M60075 Polyethylene Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade.. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate A; ASTM D1525 |
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
DuPont Bynel® 4006 Anhydride-Modified HDPE Adhesive Resin
(discontinued **) Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Ineos T50-500-196 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Shuman 210 Polyphenylene Ether Copolymer Alloy Black, Custom Colors. Good impact strength, easy processability, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer. |
|||
Vicat Softening Point | 128 °C | 262 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Chevron Phillips 1018 Extrusion Coating Resin Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Stability, Good Draw Down ResinApplications:Food Packaging, Laminations, Sealant ResinData provided by Chevron.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Chevron Phillips MarFlex® 1013 LDPE Extrusion Coating Resin Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Vicat Softening Point | 128 °C | 262 °F | |
Covestro Bayblend® KU 2-1481 Polycarbonate/ABS Blend Increased thermal stability during processing, slightly higher modulus of elasticity and slightly decreased low-temperature toughness compared to BAYBLEND T 85 MN.Information provided by Bayer.As of.. |
|||
Vicat Softening Point | 128 °C | 262 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
Vicat Softening Point | 128 °C | 262 °F | 50°C/h 50N |
Covestro Texin® 950U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, B.. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 4033 Anhydride Modified HDPE BYNEL® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Vicat Softening Point | 128 °C @Load 1.00 kg, Thickness 3.17 mm |
262 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1527 |
Diamond Polymers DIAMALOY 527 PC/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 128 °C | 262 °F | ASTM D1525 |
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Vicat Softening Point | 128 °C @Load 1.02 kg |
262 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem HE150 HDPE Monofilament Polyethylene Copolymer HE150 resin is a high-density polyethylene, copolymer of butene-1, produced by the Spherilene process. It has been specially designed for the monofilament extrusion process and provides a good balan.. |
|||
Vicat Softening Point | 128 - 220 °C | 262 - 428 °F | Average value: 183 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |