Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Vicat Softening Point | 125 °C @Load 1.00 kg |
257 °F @Load 2.21 lb |
|
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Vicat Softening Point | 125 °C @Load 5.001 kg |
257 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
Huntsman Rexell® H2109 Injection Molding LLDPE
(discontinued **) Linear-low high density injection molding.Features: High flow, good ESCR.Applications: General purpose molding, housewares.Information provided by Huntsman Corporation |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
LyondellBasell Plexar® PX2049 Extrudable Tie-Layer Resin - Anhydride Modified HDPE
(discontinued **) General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
Reliance Industries Relene D16501 Polyethylene Relene D16501 is a UV stabilized High Density Polyethylene compound with broad molecular weight distributions, suitable for producing cable duct for optic fiber and other general purpose cables. Th.. |
|||
Vicat Softening Point | 125 °C | 257 °F | (VST/B/50); ASTM D1525 |
Albis Plastics Polypropylene A 12 H-GK20/GF20 C , 20% Glass Bead/20% Glass Fiber
(discontinued **) Semi-crystalline Polypropylene Homopolymer (PPHP)Characteristics: Chemically Coupled Fiber; Good Dimensional StabilityApplications: Appliances, Furniture, Cases, Packaging and NoveltiesProcessing: I.. |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Vicat Softening Point | 125 °C @Load 5.10 kg |
257 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Vicat Softening Point | 125 °C @Load 5.00 kg |
257 °F @Load 11.0 lb |
|
LATI Latistat 83-05 POM, Impact Modified Dissipative product based on Polyamide 12 (PA12), impact modified. Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 125 °C | 257 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
Vicat Softening Point | 125 °C | 257 °F | ISO 306 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 125 °C | 257 °F | ISO 306 |
Unipetrol PE HD LITEN® MB/ML 77 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 125 °C | 257 °F | ISO 306 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
Lubrizol Estane® R195A Thermoplastic Polyurethane Type: Estane® R195A is a Shore 95A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Vicat Softening Point | 125 °C | 257 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
CPC - Vycom SANATEC® Sanitary Cutting Boards High Density Polyethylene Sanatec is a high density polyethylene specially formulated for the manufacture of quality cutting boards. Sanatec`s special surface finish insures long product life and will not dull knives. Sanate.. |
|||
Vicat Softening Point | 125 °C | 257 °F | |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |
|||
Vicat Softening Point | 125 °C @Load 5.10 kg |
257 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 125 °C | 257 °F | ASTM D1525 |
Arkema Group ORGASOL® 3502 D Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Vicat Softening Point | 125 °C | 257 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |