Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 10.3 MPa @Temperature 149 °C |
1500 psi @Temperature 300 °F |
ASTM D732 |
Greene Tweed Avalon® 56 PTFE PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use.. |
|||
Shear Strength | 10.3 MPa @Temperature 204 °C |
1500 psi @Temperature 400 °F |
ASTM D732 |
Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Shear Strength | 10.3 MPa @Temperature 25.0 °C |
1500 psi @Temperature 77.0 °F |
Die; 0.05" x 0.05" IC; Chatillon Force Gauge Model DPP-25 |
Lord Adhesives Thermosetâ„¢ MD-200 Electrically Conductive Die-Attach Adhesive This is a system with the versatility to fit a wide variety of production and performance needs. The working life allows sufficient time for short production interruption. It can be initially cured .. |
|||
Shear Strength | 10.3 MPa @Temperature 25.0 °C |
1500 psi @Temperature 77.0 °F |
Tensile; ASTM D1002 |
Lord Adhesives Thermosetâ„¢ MD-200 Electrically Conductive Die-Attach Adhesive This is a system with the versatility to fit a wide variety of production and performance needs. The working life allows sufficient time for short production interruption. It can be initially cured .. |
|||
Shear Strength | 10.34 MPa @Temperature 177 °C |
1500 psi @Temperature 350 °F |
2 hr soak, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1002 |
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character.. |
|||
Shear Strength | 10.3 MPa @Temperature -55.0 °C |
1500 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ 1838 B/A Green Two-Part Structural Adhesive Multi-purpose and Rigid bondsInformation provided by 3M |
|||
Shear Strength | 10.3 MPa @Temperature -55.0 °C |
1500 psi @Temperature -67.0 °F |
Overlap |
3M Scotch-Weld™ 1838 B/A Tan Two-Part Structural Adhesive Multi-purpose and Rigid bondsInformation provided by 3M |
|||
Shear Strength | 10.3 MPa @Temperature 121 °C |
1500 psi @Temperature 250 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Shear Strength | 10.3 MPa @Temperature 23.0 °C |
1500 psi @Temperature 73.4 °F |
Overlap, Maple |
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 10.3 MPa @Temperature 23.0 °C |
1500 psi @Temperature 73.4 °F |
Overlap, Maple |
3M Scotch-Weld™ TE031 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 10.3 MPa @Temperature 121 °C |
1500 psi @Temperature 250 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°.. |