| Category | Polymer , Thermoset , Epoxy , Epoxy Adhesive | 
| Manufacturer | 3M | 
| Trade Name | Scotch-Weld™ | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | 3M Scotch-Weld™ 2214 Regular Epoxy Adhesive.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Viscosity | 60 - 200 cP | 60 - 200 cP | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D | >= 85 | >= 85 | |
| Tensile Strength, Ultimate | 68.9 MPa | 10000 psi | |
| Elongation at Break | <= 2.0 % | <= 2.0 % | |
| Modulus of Elasticity | 5.17 GPa | 750 ksi | |
| Shear Strength |           2.76           MPa           @Temperature 177 °C  | 
                  400           psi           @Temperature 351 °F  | 
        Aluminum Overlap | 
|           4.14           MPa           @Temperature 149 °C  | 
                  600           psi           @Temperature 300 °F  | 
        Aluminum Overlap | |
|           10.3           MPa           @Temperature 121 °C  | 
                  1500           psi           @Temperature 250 °F  | 
        Aluminum Overlap | |
|           20.7           MPa           @Temperature -53.0 °C  | 
                  3000           psi           @Temperature -63.4 °F  | 
        Aluminum Overlap | |
|           31.0           MPa           @Temperature 24.0 °C  | 
                  4500           psi           @Temperature 75.2 °F  | 
        Aluminum Overlap | |
|           31.0           MPa           @Temperature 82.0 °C  | 
                  4500           psi           @Temperature 180 °F  | 
        Aluminum Overlap | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           49.0           µm/m-°C           @Temperature 0.000 - 80.0 °C  | 
                  27.2           µin/in-°F           @Temperature 32.0 - 176 °F  | 
        |
| Thermal Conductivity | 0.399 W/m-K | 2.77 BTU-in/hr-ft²-°F | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | 2.80e+13 ohm-cm | 2.80e+13 ohm-cm | |
| Surface Resistance | 9.80e+12 ohm | 9.80e+12 ohm | |
| Dielectric Constant |           10.5                     @Temperature 23.0 °C  | 
                  10.5                     @Temperature 73.4 °F  | 
        ASTM D150 | 
|           11.1                     @Temperature 60.0 °C  | 
                  11.1                     @Temperature 140 °F  | 
        ASTM D150 | |
|           16.7                     @Temperature 90.0 °C  | 
                  16.7                     @Temperature 194 °F  | 
        ASTM D150 | |
|           24                     @Temperature 104 °C  | 
                  24                     @Temperature 219 °F  | 
        ASTM D150 | |
| Dielectric Strength |           3.03           kV/mm           @Thickness 0.930 mm  | 
                  77.0           kV/in           @Thickness 0.0366 in  | 
        |
| Dissipation Factor |           0.126                     @Temperature 23.0 °C  | 
                  0.126                     @Temperature 73.4 °F  | 
        |
|           0.346                     @Temperature 90.0 °C  | 
                  0.346                     @Temperature 194 °F  | 
        ||
|           0.463                     @Temperature 60.0 °C  | 
                  0.463                     @Temperature 140 °F  | 
        ||
|           0.515                     @Temperature 104 °C  | 
                  0.515                     @Temperature 219 °F  | 
        ||
| Arc Resistance | 76 sec | 76 sec | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Appearance | Gray |