Polymer Property : Shear Strength = 2.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 2.10 MPa

@Temperature 82.0 °C
305 psi

@Temperature 180 °F
ASTM D1002-64
3M Scotch-Weld™ 3532 B/A Brown Two-Part Urethane Adhesive 3532 B/A Brown  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 20-30 minutes handling stren..
Shear Strength 2.10 MPa

@Temperature 82.0 °C
305 psi

@Temperature 180 °F
ASTM D1002-64
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren..
Shear Strength 2.10 MPa

@Temperature 82.0 °C
305 psi

@Temperature 180 °F
ASTM D1002-64
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren..
Shear Strength 2.10 MPa

@Temperature 24.0 °C
305 psi

@Temperature 75.2 °F
1/8" Birch/High-Pressure Laminate, aged 6 mo
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Shear Strength 2.10 MPa

@Temperature 24.0 °C
305 psi

@Temperature 75.2 °F
1/8" Birch/High-Pressure Laminate, aged 6 mo
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M