Mechanical Properties Metric English Comments
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
ASTM D1002-64
3M Scotch-Weld™ 3532 B/A Brown Two-Part Urethane Adhesive 3532 B/A Brown  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 20-30 minutes handling stren..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
ASTM D1002-64
3M Scotch-Weld™ 3535 B/A Off-white Two-Part Urethane Adhesive 3535 B/A Off-white  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling stren..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
ASTM D1002-64
3M Scotch-Weld™ 3549 B/A Brown Two-Part Urethane Adhesive 3549 B/A Brown  (discontinued **)
Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include long worklife adhesive, 2-4 hours handling stren..
Shear Strength 13.8 MPa

@Temperature 93.3 °C
2000 psi

@Temperature 200 °F
ASTM D732
Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Shear Strength >= 13.8 MPa

@Temperature 23.9 °C
>= 2000 psi

@Temperature 75.0 °F
Tensile lap, Al to Al
Master Bond EP46HT Epoxy Adhesive for Structural Bonding
Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f..
Shear Strength 13.8 MPa

@Temperature 149 °C
2000 psi

@Temperature 300 °F
Single Lap Shear (Metal/Metal), 0.05 psf, No conditioning
Hexcel® Redux® 330K Epoxy film adhesives for the bonding and finishing of composites
Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ 1838 B/A Tan Two-Part Structural Adhesive
Multi-purpose and Rigid bondsInformation provided by 3M
Shear Strength 13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Overlap
3M Scotch-Weld™ 1838L B/A Two-Part Structural Adhesive
Multi-purpose and Rigid bondsInformation provided by 3M
Shear Strength 13.8 MPa

@Temperature -53.0 °C
2000 psi

@Temperature -63.4 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Sc..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Sc..
Shear Strength 13.8 MPa

@Temperature 149 °C
2000 psi

@Temperature 300 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp Formula is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids,..
Shear Strength 13.8 MPa

@Temperature -40.0 °C
2000 psi

@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Steel
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap, Etched Aluminum
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Al
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature -40.0 °C
2000 psi

@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Al
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature -40.0 °C
2000 psi

@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Steel
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap, Etched Aluminum
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Al
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature -40.0 °C
2000 psi

@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Al
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature -40.0 °C
2000 psi

@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Steel
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap, Etched Aluminum
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Overlap, Abraded and Solvent Wiped Al
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Shear Strength 13.8 MPa

@Temperature -40.0 °C
2000 psi

@Temperature -40.0 °F
Overlap, Abraded and Solvent Wiped Al
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..