Mechanical Properties Metric English Comments
Shear Strength 120 MPa

@Temperature -53.9 °C
17400 psi

@Temperature -65.0 °F
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 120 MPa

@Temperature 25.0 °C
17400 psi

@Temperature 77.0 °F
+/- 45° In-Plane, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Information provided by HexCel
Shear Strength 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel
Shear Strength 120 MPa

@Temperature -54.0 °C
17400 psi

@Temperature -65.2 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, T3T095 Carbon Tape
Hexcel designation: T_095-12"-F263; Various fibersInformation provided by HexCel