Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F263 Epoxy Resin, T3T095 Carbon Tape

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F263 Epoxy Resin, T3T095 Carbon Tape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hexcel designation: T_095-12"-F263; Various fibersInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1247 MPa

@Temperature 24.0 °C
180900 psi

@Temperature 75.2 °F
Tensile Modulus 134.8 GPa

@Temperature 24.0 °C
19550 ksi

@Temperature 75.2 °F
Compressive Yield Strength 1260 MPa

@Temperature 71.0 °C
183000 psi

@Temperature 160 °F
1420 MPa

@Temperature 24.0 °C
206000 psi

@Temperature 75.2 °F
Shear Strength 75.0 MPa

@Temperature 132 °C
10900 psi

@Temperature 270 °F
Short Beam
111 MPa

@Temperature 24.0 °C
16100 psi

@Temperature 75.2 °F
Short Beam
120 MPa

@Temperature -54.0 °C
17400 psi

@Temperature -65.2 °F
Short Beam
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.01
Laminate
Dry Resin Content (%) 35-39
Prepreg
Fiber Volume (%) 55
Laminate
Flow (%) 11-24