Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 17.0 kN/m | 97.0 pli | ISO 34-1 |
PolyOne OnFlex™ S KA 40A-3S1767 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | D624 |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 9071E Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Die B |
Momentive Performance Materials TSE 221-7U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 4002 DARK GRAY Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Insulating Layer |
Fujipoly Industries Zebra® Silver Connector Fujipoly New High performance Silver Zebra connectors are constructed of alternating parallel layers of electrically conductive and nonconductive silicone elastomer. The electrically conductive laye.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Tear Strength | >= 17.0 kN/m | >= 97.0 pli | |
Silikony Polskie Polsil Gum 100/50 HTV Silicone Rubber Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei.. |
|||
Tear Strength | >= 17.0 kN/m | >= 97.0 pli | |
Silikony Polskie Polsil Gum 100/60 HTV Silicone Rubber Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: agei.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg E469 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg S561 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg S565 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Trelleborg S662 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Dow Corning HV 1650/50 SILICONE RUBBER 50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | |
Dow Corning HV 1760/65 Silicone Rubber 65 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | ASTM D624 |
ELASTO UK Dryflex® 500350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Silicone Property; ASTM D624 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Tear Strength | 17.0 kN/m | 97.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Tear Strength | >= 17.0 kN/m | >= 97.0 pli | |
Silikony Polskie Polsil Gum 213/60 HTV Silicone Rubber Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: ageing.. |