Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Silikony Polskie Polsil Gum 100/50 HTV Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Silikony Polskie
Trade Name Polsil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silikony Polskie Polsil Gum 100/50 HTV Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polsil Gum is a general purpose master batch compound, vulcanizing at high temperature after addition of vulcanizing agent. Silicone rubber obtained from Polsil® GUM shows useful properties: ageing resistance, stability of mechanical properties in the range of temperature between -500C and + 2500C, chemical resistance, good insulating properties.
Physical Properties Metric English Comments
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength at Break >= 8.00 MPa
>= 1160 psi
Elongation at Break 370 - 620 %
370 - 620 %
Tear Strength >= 17.0 kN/m
>= 97.0 pli