Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 102 kN/m | 582 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 102 kN/m | 582 pli | ISO 34-1B |
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.Main Application : ExtrusionSpecial features : Outstanding abrasion loss, excellent color stability upon weather exposure.. |
|||
Tear Strength | 102 kN/m | 582 pli | without incision; ISO 34B |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 102 kN/m | 582 pli | Die C; ASTM D624 |
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tear Strength | 102 kN/m | 582 pli | Die C; ASTM D624 |
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tear Strength | 102 kN/m | 582 pli | Graves (initial), TD; ASTM D1004 |
DuPont™ Tedlar® TWH15BL3 Low Gloss White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Tear Strength | 102 kN/m | 582 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 102 kN/m | 582 pli | Perpendicular to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6158 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 102 kN/m | 582 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1690AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 102 - 164 kN/m | 582 - 935 pli | Average value: 136 kN/m Grade Count:6 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |