Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 70.0 kN/m | 399 pli | ASTM D624 |
Multibase Multi-Flex® TPE D 4112 BLK Ash is 14%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | >= 70.0 kN/m | >= 399 pli | Method B; ISO 34 |
S&E Specialty Polymers SE900-5 PVC Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Core which meets the Ford WSKM4D689-A4Information provided by S&E Specialty Polymers |
|||
Tear Strength | 70.0 kN/m | 399 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90048 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 69.9 kN/m | 399 pli | die B; ASTM D624 |
DP7-3002 Polyurethane-based Biomedical Elastomer |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ISO 34B |
Huntsman AVALON® 80 AHT DP Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM D624 |
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene LF01090 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: general pupose film and for aminati.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM D1004 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | DIN 53515 |
Lubrizol ESTANE® 58610 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ISO 34 |
Chengdu Polyster H3303 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance at low temperatures. Moldable even in thin sections. Can be used in light-colored pro.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | Die C; ASTM D624 |
Covestro Bayflex® 110 RIM-LITE Polyurethane Elastomeric RIM, 13% Mineral Filled, MDI-based 2-Component Liquid System Contains 10% calcium silicate and 3% glass microspheres.0.15 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, .. |
|||
Tear Strength | 70.0 kN/m | 399 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers |
|||
Tear Strength | 70.0 kN/m | 399 pli | parallel; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |
|||
Tear Strength | 70.0 kN/m | 399 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |
|||
Tear Strength | 70.0 kN/m | 399 pli | DIN ISO 34-1/Bb |
BASF Elastollan SP 852 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 70.0 - 90.0 kN/m | 399 - 514 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Tear Strength | 70.0 - 90.0 kN/m | 399 - 514 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Tear Strength | >= 70.0 kN/m | >= 399 pli | ISO 34 |
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | DIN ISO 34-1/Bb |
BASF Elastollan C 85 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tear Strength | 70.0 kN/m @Thickness 0.760 mm |
399 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D1938 |
BASF Elastollan® C85A10 (917) Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 70A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 70.0 kN/m | 399 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 84A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | >= 70.0 kN/m | >= 399 pli | ISO 34 |
Austin Novel Materials Texalan® 785A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | 70.0 kN/m | 399 pli | DIN 53515 |
Lubrizol ESTANE® T5191 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 70.0 kN/m | 399 pli | DIN 53515 |
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |