Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 66.1 kN/m | 377 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 66.0 kN/m | 377 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 66.0 kN/m | 377 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 66.1 kN/m | 377 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 66.1 kN/m | 377 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tear Strength | 66.0 kN/m @Thickness 0.760 mm |
377 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D1938 |
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tear Strength | 66.0 kN/m @Thickness 0.760 mm |
377 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D-1938 |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tear Strength | 66.0 kN/m | 377 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Carbon Black, N-550 (FEF) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 66.0 kN/m @Thickness 0.760 mm |
377 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D-1938 |
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tear Strength | 66.0 kN/m @Thickness 0.760 mm |
377 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D-1938 |
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tear Strength | 66.0 kN/m @Thickness 0.760 mm |
377 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D1938 |
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |