Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 39.0 - 49.0 kN/m | 223 - 280 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8502 BLK The fogging test value is 90% according to ASTM SAE-J275. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 39.1 kN/m | 223 pli | Die C |
NEU NeuSoft™ 596-50A Medical Ether TPU / SBC blend |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Type C; ASTM D624 |
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Tear Strength | 39.0 - 45.0 kN/m | 223 - 257 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 6K Polytetrafluoroethylene Coated Kevlar Fabric PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 6040 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 39.1 kN/m | 223 pli | Die B |
Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber ShinEtsu KEG200170 is a very fast cure liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KEG20.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2002-50A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tear Strength | 39.1 kN/m | 223 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 75-LR-9 TPE Product Description: StarTUFF TF 75-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | ASTM D624 |
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 39.0 kN/m | 223 pli | ASTM D2240 |
UBE UBEPOL BR150B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.1 kN/m | 223 pli | Die B, no post cure; ASTM D624 |
Multibase C6-180 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 39.0 kN/m | 223 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |