Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 28.0 kN/m | 160 pli | ISO 34-1 |
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | D624 |
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 28.0 kN/m | 160 pli | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 221-73 W175 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic UV grade elastomer designed for thin wall extrusion applications with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and c.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 73°F; ASTM D624 |
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and desig.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-9 TPE Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® SG33-05(R) Industrial Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Initial Tear Strength |
Saint-Gobain CHR® SG35-05(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 6 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Sumitomo Chemical ESPOLEX® 3675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
Dow Corning C6-530 LIQUID SILICONE RUBBER KIT Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and partsInformation provided by Dow Corning |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
Dow Corning HV 1551/70P 40 Shore hardness low viscosity injection mouldable liquid silicone rubber with high tear strength, high elongation and a fast cure speed.Information provided by Dow Corning |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
ELASTO UK Dryflex® 502650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Across Flow, Method Bb, Angle (Nicked); ISO 34-1 |
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Diamond Polymers Softflex® SF 4494 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 28.0 kN/m | 160 pli | ASTM D624 |
Diamond Polymers Softflex® SF 8900 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 28.0 kN/m | 160 pli | |
Axiall 8740 Moldings & Extrusions Flexible PVC General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | 28 kN/m at 23°C. Value at 100°C is 13 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 38-034 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclaimer: A.. |
|||
Tear Strength | 28.0 kN/m | 160 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6250 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |