Material Notes:
Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Viscosity 9400 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
9400 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 45

@Time 10.0 sec
45

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 6.69 MPa

@Time 7200 sec
970 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 715 %

@Time 7200 sec
715 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00169 GPa

@Time 7200 sec
0.245 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 28.0 kN/m
160 pli
ASTM D624
Descriptive Properties Value Comments