Mechanical Properties Metric English Comments
Tear Strength 98.0 kN/m
559 pli
ASTM D624
Multibase Multi-Flex® TPE A 9402-SR BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 98.0 kN/m
559 pli
ASTM D624-95
Multibase Multi-Flex® TPO 1047-3000
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Tear Strength 98.0 kN/m
559 pli
ASTM D624-95
Multibase Multi-Flex® TPO 1047-3000 COMPOUND
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Tear Strength 98.0 kN/m
559 pli
ASTM D624
Toyobo PELPRENE™ P40H Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Tear Strength 98.0 kN/m
559 pli
ASTM D624
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit
Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo.
Tear Strength 98.0 kN/m
559 pli
ASTM D624
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant
Features: Polyester TPE, Weather-resistantInformation provided by Toyobo.
Tear Strength 98.0 kN/m
559 pli
ASTM D624
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point
Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo.
Tear Strength 98.0 kN/m
559 pli
ASTM D624-95
Multibase Multi-Flex® TPO D 5308 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302.Data provided by Multibase.