Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 70.1 kN/m | 400 pli | Die C, 51 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90215 Polyvinyl Chloride, Flexible (PVC, Flexible) Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne |
|||
Tear Strength | 70.1 kN/m | 400 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tear Strength | 70.1 kN/m | 400 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 70.1 kN/m | 400 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 70.1 kN/m | 400 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 70.1 kN/m | 400 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 |
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Tear Strength | 70.1 kN/m | 400 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-280A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black Information provided by ITW Devcon |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 DIE C |
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low .. |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black Information provided by ITW Devcon |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 |
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Initial Tear Strength |
Saint-Gobain CHR® SG03-14(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Initial Tear Strength |
Saint-Gobain CHR® SG05-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Initial Tear Strength |
Saint-Gobain CHR® SG06-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Initial Tear Strength |
Saint-Gobain CHR® SG13-14(R) High Performance Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Initial Tear Strength |
Saint-Gobain CHR® SG15-14(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Initial Tear Strength |
Saint-Gobain CHR® SG16-14(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Warp/Longitudinal direction; ASTM D1000 |
Saint-Gobain COHRlastic® 3032 Low Temperature Flexibility Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® q-GUARD® 18 Insulation Jacketing Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fibergl.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® TCK® 1590 High-Strength Leno Weave Open Mesh Belting Material Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid .. |
|||
Tear Strength | 70.1 kN/m | 400 pli | |
Saint-Gobain COHRlastic® CF4444 Reversion Resistant Reinforced Solid Rubber Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction.. |
|||
Tear Strength | 70.1 kN/m | 400 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® TCK® 1000 High-Strength Leno Weave Open Mesh Belting Material Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid .. |
|||
Tear Strength | 70.1 kN/m | 400 pli | ASTM D624 |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |