Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 63.8 kN/m | 364 pli | |
Network Polymers Softflex® 8103 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 63.8 kN/m | 364 pli | Die C; ASTM D1004 |
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 63.8 kN/m | 364 pli | Die C; ASTM D1004 |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 63.8 kN/m | 364 pli | Die C; ASTM D1004 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tear Strength | 63.8 kN/m | 364 pli | Die C; ASTM D1004 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |