Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 42.1 kN/m | 240 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tear Strength | 42.1 - 49.1 kN/m | 240 - 280 pli | ASTM D624 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tear Strength | 42.1 kN/m | 240 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 42.1 kN/m | 240 pli | ASTM D624 |
Multibase Multi-Flex® A 7005 C TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Tear Strength | 42.1 kN/m | 240 pli | ASTM D624 |
Multibase Multi-Flex® A 8502 A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 42.1 kN/m | 240 pli | Die C; ASTM D624 |
Teknor Apex Monprene® MP-2156 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | ASTM D624 |
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Tear Strength | 42.1 kN/m | 240 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7010-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 42.1 kN/m | 240 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | |
Dow Corning C6-150 ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | |
Dow Corning C6-165 ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | |
Dow Corning C6-540 LIQUID SILICONE RUBBER KIT Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and parts.Information provided by Dow Corning |
|||
Tear Strength | 42.1 kN/m | 240 pli | |
Dow Corning SILASTIC® Q7-4780 BIOMEDICAL GRADE ETR ELASTOMER, KIT Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.I.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | Die C; ASTM D3575 Suf. G |
Monmouth Rubber & Plastics Superbounce 90 NEO/SBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tear Strength | 42.1 kN/m | 240 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3880E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-4080 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInforma.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |
|||
Tear Strength | 42.1 kN/m | 240 pli | ASTM D1004 |
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.Tygon® Ultra Chemical Resistant Tubing is virtually unaffec.. |
|||
Tear Strength | 42.1 kN/m | 240 pli | die C; ASTM D624 |
PB1100-75 Polyurethane-based Biomedical Elastomer |