Material Notes:
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastomers. These materials are ideal for applications requiring flexibility over a wide temperature range, excellent colorability, broad processing capability and durability.Description/Features:High Performance Thermoplastic ElastomerNaturalApplications: Multi-PurposeFDA (Food contact)Processing Method: ExtrusionInformation provided by PolyOne Corporation
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
10 Sec; ASTM D2240
84
84
Instant; ASTM D2240
Tensile Strength, Yield 10.1 MPa
1470 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
7.24 MPa

@Strain 300 %
1050 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 620 %
620 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 42.1 kN/m
240 pli
Die C (graves), 20 in/min; ASTM D624