Material Notes:
Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded parts.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Tensile Strength, Ultimate 8.07 MPa
1170 psi
Elongation at Break 940 %
940 %
Tear Strength 42.1 kN/m
240 pli