Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 47.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
cond.; ISO 6603-2
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Puncture Energy 65.0 J

@Temperature 23.0 °C
47.9 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral
PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Apec® 1703 Polycarbonate
UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Apec® 1800 Polycarbonate
Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Apec® 1803 Polycarbonate
UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2467 Polycarbonate
ISO 7391-PC,MFLR,(,,)-18-9Global gradeFormerly Makrolon DP1-1870MVR (300 °C/1.2 kg) 19 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmLow viscosityUV stabilizedEasy r..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2556 Polycarbonate
MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2558 Polycarbonate
ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2656 Polycarbonate
ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2806 Polycarbonate
ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2856 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2865 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt tempe..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem..
Puncture Energy 65.0 J
47.9 ft-lb
Puncture energy +23°C
Covestro Makrolon® 3158 Polycarbonate
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated..
Puncture Energy 65.0 J
47.9 ft-lb
ISO 6603-2
Covestro Makrolon® 3206 Polycarbonate
ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade
MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 6457 Polycarbonate, Flame Retardant Grade
MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmUV stabilizedeasy releaseinjection moldingavailable in transparent, translucent and opaque colorsPreprocessingMax. Water content
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® AG2677 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transparent colors on..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® AL2447 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LTG2623 Polycarbonate
PreprocessingMax. Water content
Puncture Energy 65.0 J
47.9 ft-lb
ISO 6603-2
Covestro Makrolon® Rx1805 Polycarbonate
ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 1243 Polycarbonate
ISO 7391-PC,ELS,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityBranchedUV stabilizedEasy releaseAvailable in color code 550111onlyMulti wall sheet/profilesPreprocessi..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® 2456 Polycarbonate
ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® DP1-1843* Polycarbonate
ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2..
Puncture Energy 65.0 J
47.9 ft-lb
ISO 6603-2
Covestro Makrolon® KU1-1230* Polycarbonate
ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® LQ2687 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t..
Puncture Energy 65.0 J

@Temperature -30.0 °C
47.9 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Covestro Makrolon® Rx1452 Polycarbonate
ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie..
Copyright © lookpolymers.com All Rights Reserved