Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 46.0 J | 33.9 ft-lb | ISO 6603-2 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |
|||
Puncture Energy | 46.0 J | 33.9 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Puncture Energy | 46.0 J @Temperature -40.0 °C |
33.9 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Puncture Energy | 46.0 J | 33.9 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Puncture Energy | 46.0 J @Temperature -40.0 °C |
33.9 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Puncture Energy | 46.0 J | 33.9 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Puncture Energy | 46.0 J @Temperature -40.0 °C |
33.9 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Puncture Energy | 46.0 J | 33.9 ft-lb | ISO 6603-2 |
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e.. |
|||
Puncture Energy | 46.0 J | 33.9 ft-lb | ISO 6603-2 |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |