Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.50 - 4.80 J @Temperature -30.0 - -30.0 °C |
1.84 - 3.54 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 3.10 J Grade Count:4 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Puncture Energy | 2.50 - 4.80 J @Load <=78.5 kg |
1.84 - 3.54 ft-lb @Load <=173 lb |
Average value: 3.10 J Grade Count:4 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Puncture Energy | 2.50 J @Temperature -30.0 °C |
1.84 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow) |
|||
Puncture Energy | 2.50 J @Temperature -30.0 °C |
1.84 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow) |
|||
Puncture Energy | 2.50 J @Temperature -30.0 °C |
1.84 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
Puncture Energy | 2.50 J @Temperature -30.0 °C |
1.84 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
Puncture Energy | 2.50 J | 1.84 ft-lb | 66N; ASTM D5748 |
Borealis FT5230 Low Density Polyethylene FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: .. |
|||
Puncture Energy | 2.50 J | 1.84 ft-lb | 66N; ASTM D5748 |
Borealis FT5231 Low Density Polyethylene FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d.. |
|||
Puncture Energy | 2.50 J | 1.84 ft-lb | 66N; ASTM D5748 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Puncture Energy | 2.50 J | 1.84 ft-lb | 66N; ASTM D5748 |
Borealis FT5236 Low Density Polyethylene FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic.. |
|||
Puncture Energy | 2.50 J @Temperature -30.0 °C |
1.84 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |