Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Impact; 52 J; 2.1 mm; ISO 6603 |
Propex Fabrics Curv™ C100A Polypropylene/Polypropylene Thermoformable Composite Curv™ key features include weight savings, total recyclability, no glass content, thermoformable, high impact strength, inertness, and abrasion resistance.Data provided by BP Amoco; Curv was spun o.. |
|||
Puncture Energy | 40.0 - 71.0 J | 29.5 - 52.4 ft-lb | Average value: 49.1 J Grade Count:12 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | ISO 6603-2 |
Lanxess Pocan® B 1300 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture energy -30°C |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture energy +23°C |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture energy -30°C |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture energy -30°C |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture energy +23°C |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture energy -30°C |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | ISO 6603-2 |
Borealis HG430MO Polypropylene HG430MO is a polypropylene homopolymer intended for injection molding. This polymer product is characterized by a superior impact resistance. This grade has ductile failure in falling weight impact .. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar AN011 Copolyester Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | At Max load; ASTM D3763 |
Eastman Eastar CN005 Copolyester, High Flow Grade Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | At Max load; ASTM D3763 |
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Puncture Energy | 40.0 J | 29.5 ft-lb | Puncture Resistance @Max Load, 0°C; ASTM D3763 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Puncture Energy | 40.0 J @Temperature -30.0 °C |
29.5 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Apec® DP1-9389/5 Polycarbonate Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content |