Mechanical Properties Metric English Comments
Puncture Energy 2.80 - 2.80 J

@Temperature -30.0 - -30.0 °C
2.07 - 2.07 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.80 J Grade Count:1
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Puncture Energy 2.80 J
2.07 ft-lb
ISO 6603-2
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® AKV 50 H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow)
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow)
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
Puncture Energy 2.80 J

@Temperature -30.0 °C
2.07 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber