Mechanical Properties Metric English Comments
Flexural Modulus 0.400 - 3.00 GPa
58.0 - 435 ksi
Average value: 2.19 GPa Grade Count:5
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 0.696 - 3.00 GPa
101 - 435 ksi
Average value: 1.50 GPa Grade Count:41
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
Flexural Modulus 0.814 - 3.00 GPa
118 - 435 ksi
Average value: 1.84 GPa Grade Count:43
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Flexural Modulus 2.50 - 3.00 GPa
363 - 435 ksi
ASTM D790
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 2.70 - 3.00 GPa
392 - 435 ksi
ASTM D790
3D Systems Accura® 60 Plastic for SLA® Systems
Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr..
Flexural Modulus 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D790
Chang Chun Plastic PBT2000 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.
Flexural Modulus 2.70 - 3.00 GPa
392 - 435 ksi
ASTM D790
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer
Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView ..
Flexural Modulus 0.700 - 3.00 GPa
102 - 435 ksi
Average value: 1.45 GPa Grade Count:42
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..