Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D790 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D790 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D790 |
Techmer ES Plaslube® NY-1/MS/5 BK223 PA66 |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D790 |
Techmer ES Plaslube® NY-1/MS/5 NAT PA66 |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D638 |
ACC EP QSZ EPI Engineered Polymers Quick Set Epoxy with Zinc EP QSZ Quick Set Epoxy with Zinc, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s (Volatile Organic Compound), self-leveling modified epoxy. This versatile new gene.. |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D638 |
ACC EP WQS EPI Engineered Polymers Water Base Quick Set Epoxy EP WQS Water Base Quick Set, “Powered by Reactamine® Technology”, is a two component 60% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast.. |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D790 |
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati.. |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D-790 |
Axiall 8240 Rigid PVC, Extrusion Georgia Gulf 8240 is a general-purpose rigid PVC extrusion compound designed for applications requiring the following properties: Rigidity/StiffnessGlossImpact Strength & ToughnessFlame RetardantCh.. |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | ASTM D638 |
ACC EP QS EPI Engineered Polymers Quick Set Epoxy EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure.. |
|||
Flexural Modulus | 3.34 GPa | 485 ksi | Tangent; ASTM D790 |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |